  • Abstract

    Problematic issues with electrically inert binders have been less serious in the conventional lithium-ion batteries by virtue of permeable liquid electrolytes (LEs) for ionic connection and/or carbonaceous additives for electronic connection in the electrodes. Contrary to electron-conductive binders used to maximize an active loading level, the development of ion-conductive binders has been lacking owing to the LE-filled electrode configuration. Herein, we represent a tactical strategy for improving the interfacial Li+ conduction in all-solid-state electrolyte-free graphite (EFG) electrodes where the solid electrolytes are entirely excluded, using lithium-substitution-modulated (LSM) binders. Finely tuning a lithium substitution ratio, a conductive LSM–carboxymethyl cellulose (CMC) binder is prepared from a controlled direct Na+/Li+ exchange reaction without a hazardous acid involvement. The EFG electrode employing LSM with a maximum degree of substitution of lithium (DSLi) of ∼68% in our study shows a considerably higher rate capability of 1.05 mA h cm–2 at 1 C and a capacity retention of ∼61.9% after 200 cycles at 0.5 C than those using sodium-CMC (Na-CMC) (0.78 mA h cm–2, ∼49.5%) and LSM with ∼35% lithium substitution (0.93 mA h cm–2, ∼55.4%). More importantly, the correlation between the phase transition near the bottom region of the EFG electrode and the state of charge (SOC) is systematically investigated, clarifying that the improvement of the interfacial conduction is proportional to the DSLi of the CMC binders. Theoretical calculations combined with experimental results further verify that creating the continuous interface through abundant pathways for mobile ions using the Li+-conductive binder is the enhancement mechanism of the interfacial conduction in the EFG electrode, mitigating serious charge transfer resistance.

  • 댓글목록

    등록된 댓글이 없습니다.


    사이트 정보

    연세대학교 DIGITAL TWIN BATTERY LABORATORY

    • 주소 : 서울특별시 서대문구 연세로50, 연세대학교 제1공학관 A155호
    • TEL : +82-2-2123-7794
    • FAX : +82-2-312-6401

    Copyright (C) 2024 YonseiUniversity. All rights reserved. Designed By (주)드림위드컴퍼니